TECHNET Archives

October 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Lee parker <[log in to unmask]>, TechNet E-Mail Forum <[log in to unmask]>
Date:
Thu, 19 Oct 2006 11:29:03 +0530
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
From:
Anil Kher <[log in to unmask]>
X-cc:
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="windows-1250"
MIME-Version:
1.0
Parts/Attachments:
text/plain (177 lines)
Sorry for rehashing the obvious but am trying to get the problem.

There is copper migration after thermal cycling on top of Gold. The gold
thickness varies from 1 to 0.1 um and Nickel shows porosity.

If it is electroplated Ni/Au - it is not necessary to find Cobalt. However
it is unlikely to get 1 um and 0.1 um on the same board in electroplating.
Max 0.1 to 0.2 um.

If ENIG we could have LPISM residues which obstructed ENI and lead to
porosity and uneven Gold deposit and hence failure. (cannot comprehend
chemistry behind what George says of high gold where nickel skips and copper
available - but if the guru says it must be).

To me the problem in either case is unclean base or a terribly unbalanced
ENIG.

Anil Kher
micro interconnexion pvt. ltd
D3-12A, Corlim Industrial Estate
Corlim, Ilhas , Goa , India 403110
tel: 91-832-2284209/337. fax 2284209/2285271
e mail: [log in to unmask]
Leaders in Gold plated PCBs - selective/ cob
an ISO 9001-2000 Company

-----Original Message-----
From: Lee parker [mailto:[log in to unmask]]
Sent: Thursday, October 19, 2006 1:53 AM
Subject: Re: ENIG problem

This could very likely be Flash Gold which is electroplated gold and nickel.
If this is the case, all of the outer traces will be plated with soft gold
over nickel; the soldermask will rest on the gold coating. You may want to
have the supplier's local rep have cross sections made of the traces at a
lab of your choosing.

Best regards

Lee

J. Lee Parker, Ph.D.
JLP Consultants LLC
804 779 3389




----- Original Message -----
From: "Hfjord" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Wednesday, October 18, 2006 11:58 AM
Subject: Re: [TN] ENIG problem


> Not one single count of Cobalt.
> Inge
>
>
> ----- Original Message -----
> From: "R Sedlak" <[log in to unmask]>
> To: <[log in to unmask]>
> Sent: Wednesday, October 18, 2006 1:09 AM
> Subject: Re: [TN] ENIG problem
>
>
> > Ingemar:
> >
> > I have a suspicion you may have found the answer...
> > Thick gold can only mean electroplated gold... electroplated gold is
> > often alloyed (think Cobalt is most common alloying metal)... which
> > undoubtedly would make bonding difficult.... remember, in
> > electroplating gold, pure gold is often referred to as "soft
> > gold".... the alloying metals are present to harden the gold...
> > which has to interfere with bonding...
> >
> > And from the comments about appearance, it may well not be well alloyed.
> >
> > Rudy Sedlak
> > RD Chemical Company
> >
> > "Ingemar Hernefjord (KC/EMW)" <[log in to unmask]> wrote:
> > Hi amigos,
> > I should never said that we had no ENIG problems. Now we seem to
> > have one. Chinese board supplier. Problems with heavy wire aluminum
> > bonding on the ENIG pads. Too low pull test values. Possible reason:
> > pad surface invaded by copper particles after the
> > bake/reflow/mounting. Sending picture to Mr Yoda. Never seen this
> > before. Gold is too thick for being ENIG (>1um), Nickel about 6um.
> > Can't see how Copper could diffuse to the surface so rapidly and at
> > those low temperatures which are typical for a general assembly
> > process. Any clue? Graham? You seem to be sitting at the keyboard just
now.
> > Ingemar Hernefjord
> > SAAB MICROWAVE SYSTEMS
> >
> > ---------------------------------------------------
> > Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> > To unsubscribe, send a message to [log in to unmask] with following
> > text in the BODY (NOT the subject field): SIGNOFF Technet To
> > temporarily halt or (re-start) delivery of Technet send e-mail to
> > [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE
> > mailing per day of all the posts: send e-mail to
> > [log in to unmask]: SET Technet Digest Search the archives of previous
> > posts at:
> > http://listserv.ipc.org/archives
> > Please visit IPC web site
> > http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> > for additional information, or contact Keach Sasamori at
> > [log in to unmask] or 847-615-7100 ext.2815
> > -----------------------------------------------------
> >
> >
> >
> > ---------------------------------
> >
> > ---------------------------------------------------
> > Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> > To unsubscribe, send a message to [log in to unmask] with following
> > text in the BODY (NOT the subject field): SIGNOFF Technet To
> > temporarily halt or (re-start) delivery of Technet send e-mail to
> > [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE
> > mailing per day of all the posts: send e-mail to
> > [log in to unmask]: SET Technet Digest Search the archives of previous
> > posts at:
> > http://listserv.ipc.org/archives
> > Please visit IPC web site
> > http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> > for additional information, or contact Keach Sasamori at
> > [log in to unmask] or 847-615-7100 ext.2815
> > -----------------------------------------------------
> > Get your email and more, right on the  new Yahoo.com
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
> unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
> or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
> per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at
> [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

--
No virus found in this outgoing message.
Checked by AVG Free Edition.
Version: 7.1.408 / Virus Database: 268.13.4/480 - Release Date: 10/17/2006

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2