TECHNET Archives

January 2011

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Fri, 14 Jan 2011 00:06:47 +0100
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Inge <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; format=flowed; charset="iso-8859-1"; reply-type=original
From:
Parts/Attachments:
text/plain (50 lines)
I bought a digital temperature equipment, consisting of a inhouse table unit 
and a outdoors unit. Cost = 25 USD. Cheap? Yes. But let's have a look on 
inside after the problem, which started just a few weeks. You can read the 
inside temperature, clock works, date works, and you can use the alarm and 
shift between the four channels, but the receiver does not take in the 
signals from the little sender on the  wall any more. I dismantled the box 
and marvelled when I saw the shit I payed for. It's a wonder that there are 
any functions working at all! Now, what caused the dead receiver was a flow 
of iron from one screw (upper left  corner ) . There is a bridge of 
corrosion products  (brown and green) from the screw to the thermistor (RT) 
continuing to the rest of the circuitry.  When I washed the card and dried 
it, the reciever worked again,

Now, folks, here comes a question for the sharp TNetters:

"How can the screw be so rusty and deliver iron ions when it's not connected 
to anything? It's just torqued into the plastic body. The other screws are 
identical, but  have not been involved in anything. "

The box has been on the kitchen table and has not been exposed to humidity 
or any else abnormal condition.

The two 1.5 V batteries are removed on the pics.

Hope the gregorian Steve will help me with the photos.

/Inge








______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2