Kevin:
You ask some pretty general questions, the answers for them, will vary with
the compound.
In general, Aluminum is a highly reactive metal, and will strip the halides
from the organics, while releasing energy.
Al + R-Cl -->> AlCl3 + R-
Many of the solvents had inhibitors to prevent/minimize this from occurring.
How fast and what circumstances accelerated this varied.
It is clear that water probably accelerates, and heat certainly does.
My suspicion is that the fluocarbons are the most stable, with chlorinated
being less, and brominated even less, so keep the Mt. Dew from Aluminum!
Rudy Sedlak
RD Chemical Company
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|