TECHNET Archives

September 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Wed, 6 Sep 2006 07:56:59 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Tom Stearns <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="iso-8859-1"
From:
Tom Stearns <[log in to unmask]>
Parts/Attachments:
text/plain (36 lines)
John:

Two  reasons for overcoating a flex/solder joint interface:

1. Insulation
2. Strain relief

Two considerations:

1. Adhesion to the flex dielectric
2. Stress concentration

Most flex is polyimide-based; polyimides are very difficult to adhere.
Surface  must be extremely clean and receptive to the overcoating  material.
Pay considerable attention to the strain relief/stress concentration
issue---be sure that the added material doesn't worsen the situation!

A slightly flexiblized system is likely to be your best choice both because
these systems tend to show higher adhesion because slightly forgiving, and
because they tend to spread stress.

Tom Stearns
3 Brander Court
Nashua NH 03063
603 889 2522

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2