Electroless Gold works pretty well. Solderstation One used to
provide the service. Now Superior metal finishing is supplying the
service.  Superior is somewhere in Los Angeles, CA. 714-524-8525

pete

On 17 Mar 03, at 8:46, Mike Kuczynski wrote:

> Thanks to all for the wirebonding information last week. Here's a
> follow-up question.
>
> Is there another way to get 30-50 microinches of soft gold on an FR4
> board, besides electroplating?
> (Current vendor want to add a buss-bar to the board w/ connection to each
> pad)
> .062" thk bd, .0035/.0035 trace/spacing, 3" x 3" in size
>
>


Peter Menuez
QA Manager
Proto Circuit, Inc.
330-572-3400
[log in to unmask]

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2