TECHNET Archives

December 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Transfer-Encoding:
7bit
Sender:
Subject:
From:
James Kittel <[log in to unmask]>
Date:
Tue, 8 Dec 1998 07:19:08 -0700
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (84 lines)
Steve,
Thanks for the excellent info, especially BGA preforms.  Oh, if I call
Indium to ask about their balls, I will say I am Steve Gregory (Har
Har).

>-----Original Message-----
>From:  Stephen R. Gregory [SMTP:[log in to unmask]]
>Sent:  Monday, December 07, 1998 3:42 PM
>To:    [log in to unmask]
>Subject:       Re: [TN] Solder Balls for BGA's
>
>In a message dated 12/7/98 12:53:36 PM Pacific Standard Time,
>[log in to unmask] writes:
>
><< Try Indium Corporation at 315 853 4900
>
> Regards
> Gerard O'Brien
> Photocircuits
>
> -----Original Message-----
> From:   James Kittel [SMTP:[log in to unmask]]
> Sent:   Monday, December 07, 1998 10:12 11:05
> To:     [log in to unmask]
> Subject:        [TN] Solder Balls for BGA's
>
> Anyone know of a source for replacement eutectic solder balls for BGA's?
>  I need 0.0295 inch dia balls (0.75 mm).
>
> Thanks,
> Jim Kittel >>
>
>Hi Jim!
>
>     One other place you can check is Winslow Automation, they've got BGA
>preforms and may have your pattern. Their phone number is: (408) 526-1213.
>Believe you me, working with their preforms is a heck of a lot easier than
>anything else I've tried using to re-ball BGA...and they're really reasonable
>as far as price goes.
>
>-Steve Gregory-
>
>P.S. Giving a number to check whether or not a company has certain sized
>balls
>        brings fond memories of back when I was a kid creating
>mischief...(GRIN).
>        Does anybody relate to this? This is the 90's style..(yer lyin' if
>ya'
>say ya'
>        don't...hehehe)
>
>                      Ring, ring, ring..."Hello, Indium corporation..."
>                     "Yes, I was wondering, do you have .75mm diameter
>balls?"
>                     "You do? Well what sized jock strap do ya' wear? HAR!
>HAR!" *..click..*
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
>text in the body:
>To subscribe:   SUBSCRIBE TechNet <your full name>
>To unsubscribe:   SIGNOFF TechNet
>################################################################
>Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
>for additional information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or
>847-509-9700 ext.312
>################################################################
>

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2