Hi Bev! There is a fairly large set of industry data on the solder joint
reliability problems induced by Gold/Tin intermetallic  (Au4Sn) formation
and a smaller data set on the solder joint reliability problems induced by
Silver/Tin intermetallic  (Ag3Sn) formation.  See Klein Wassink's book ISBN
0-901150-24-X. I would expect that if you have both intermetallic species
in a solder joint it just would not be a "good" thing. The use environment
of the assembly would also play a role in just "how much" intermetallic
degradation would be allowable. Tough question - good luck.

Dave Hillman
Rockwell Collins
[log in to unmask]




Bev Christian <[log in to unmask]>@IPC.ORG> on 04/16/2001 08:33:58 AM

Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
      to Bev Christian <[log in to unmask]>

Sent by:  TechNet <[log in to unmask]>


To:   [log in to unmask]
cc:

Subject:  [TN] Embrittlement


Good morning!
Here is a met. question to start off the day.

We know that if we have over 4% gold in a 63/37 tin lead solder joint we
risk gold induced embrittlement because of the production of a  significant
amount of the tin/gold intermetallic.  It is also common practise to use a
slight variation of the eutectic solder with a 62/36/2 Sn/Pb/Ag
composition.
We also know that gold and silver are 100% soluble in each other.  My
question: if the final tin/lead based solder joint composition has a
COMBINED noble metal percentage in the 4% range how bad is that for solder
joint reliability?

regards,
Bev Christian
Research in Motion

---------------------------------------------------------------------------------

Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2