For round No CC areas a dot larger than the required area
should be fine, making sure all solder joints adjacent are Cced. For
linear areas, a tolerance of - 0/+50 mils is doable, again making sure
all SJ are covered. It translates to a target of the area plus 25 mils
with a tolerance of plus or minus 25 mils. Some people ask for the moon,
but we need to be practical and not spent too much time on masking.
Unless of course they are willing to fork out sufficient dough.
Ramon
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Graham Collins
Sent: Monday, February 05, 2007 9:22 AM
To: [log in to unmask]
Subject: Re: [TN] Conformal Coating Masking Requirements
Hi Amol!
We deal with multiple customers here. We request drawings specify
either tolerances, or a verbal description of the area e.g. "mating
surfaces of connectors". We have some instances where the drawing has a
cross-hatched area and a drawing note that says to mask approximately
where shown.
We have had problems where drawings only specify a dimensioned keep-out
area, and the general tolerance for the drawing is something small - so
it says to mask something like .25" +- .005" - not my idea of a good
time. When we get drawings like that we submit change requests to
loosen the tolerance for the keep-out area.
Always fun.
regards,
Graham Collins
Process Engineer,
L-3 Communications Electronic Systems Inc.
Halifax
(902) 873-2000 ext 6215
>>> [log in to unmask] 02/05/07 10:06AM >>>
Dear all,
Since we are on the topic of conformal coating, I wanted to get a feel
for how conformal coating masking requirements are being requested by
the customer and being handled by the manufacturers. The customer
drawing usually states the type of CC to be used and the keep-out areas
for the coating (usually location Ids on the board). When one is masking
on the keep-out areas, what tolerances are being used around the
keep-out areas?.......IPC 610 D only states that there should be no CC
on keep-out areas, and therefore by logical deduction, also assumes that
all areas except the keep-out areas are to be covered by coating.
Obviously, there are practical limitations to this requirement. For
example, a test via is a keep-out area, but the trace running from the
via is not. Is everybody out there JUST masking the via, and then doing
manual touch up on the extra keep-out area if any, afterwards? If one
goes too close, the coating flows on the keep-out area, and if one
leaves some space, you are violating IPC specs! .,..........I am
thinking along the lines of asking customers to specify a tolerance for
the keep-out areas as some of them are very particular about this issue.
Requesting your thoughts, current best practices etc
Regards,
Amol
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Barmuta, Michael
Sent: Friday, February 02, 2007 6:27 PM
To: [log in to unmask]
Subject: Re: [TN] Humiseal Masking Tape Residues/latex peelable
Hi Steve: Well let's think about this again. Some food for thought......
* I assume your are using the HT500 tape. Have you tried a
different tape? In addition to the HT500 we also use Shercon's
"Conformal Coat" tape. It has a different backing and adhesive.
* Possible compatibility issue with the soldermask? Have you
tried
the HT tape on a different soldermask and a different lot of boards with
the same soldermask?
* Possible flux or wash residue or moisture interactions? Are the
boards washed and thoroughly dried prior to CC?
* Are you absolutely sure that the masking tape was on the board
for only an hour?
* Could the tape been applied to a hot board? Locking in the
adhesive?
* Since the initial problem have you built some up "by the book".
Same problem?
Have a Good Weekend
Mike Barmuta
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Friday, February 02, 2007 12:19 PM
To: [log in to unmask]
Subject: Re: [TN] Humiseal Masking Tape Residues/latex peelable
Hi Michael!
Believe it or not, it is adhesive. When we go to remove the residue,
it's real gummy and sticky...just like the tape adhesive. Take a look at
this picture:
http://stevezeva.homestead.com/files/Tape_Adhesive.jpg
It's a piece of the tape that I've taken and carefully scrapped at on
the sticky (adhesive) side until I've gotten to the carrier part of the
tape, and the carrier part of the tape is actually clear...it's the
adhesive that's tan. I looked at the MSDS and the tape is actually a
polyethyleneterephthalate film, and the adhesive is listed as a rubber
adhesive.
Like I said, I've never had this problem before.I used Humiseal tape
over at LaBarge while I was there, and switched our conformal coat area
over to the tape since I've been here at OAI. I've just now started
seeing the problem.
The tape doesn't stay on the board for more than 1-hour after spraying
before we remove it. The one weird thing that I am seeing is that I only
see the residues at places like in my first picture where we've masked
over PTH locations where the tape is completely on the PCB soldermask.
I
don't see the residues on places where the tape is over the tin/lead
board finish, or metal (like the connector sheilds on press-fit
connectors.
-Steve Gregory-
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Barmuta, Michael
Sent: Friday, February 02, 2007 12:34 PM
To: [log in to unmask]
Subject: Re: [TN] Humiseal Masking Tape Residues/latex peelable
Steve: I would agree with Doug. By the appearance and color of the
residue it looks like the tape itself.
We are also using Humiseal's tape, in both strip and dot form. We have
not seen any issues with adhesive residue. One thing we monitor closely
is how long the tape is on the board after application. After
application we wait for two hours then remove the tape. Longer times can
cause release problems with the tape.
Hi Kenny: We used to use a liquid latex maskant but found it messy and
cumbersome to use. Have you considered preformed masking aids or tape?
Or is the design such that they won't work?
Check with Chemtronics they had a peelable latex product, Chemmask HV.
The rheology of the formulation was very good, preventing it from
flowing or spreading out after application.
Regards
Michael Barmuta
Staff Engineer
Fluke Corp.
Everett WA
425-446-6076
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Friday, February 02, 2007 9:31 AM
To: [log in to unmask]
Subject: [TN] Humiseal Masking Tape Residues...
Hi All!
I have a conformal coat masking problem too along with KennyB. We're
getting residues from the Humiseal tape we're using when we remove the
tape.
We're coating the boards with 1B31, and we don't bake the boards with
the tape on. We take the tape off right after we spray the board.
Check
out:
http://stevezeva.homestead.com/files/Tape_Residues.jpg
I've not had this problem with Humiseal tape before. Our customer is
rejecting the boards and it is quite time consuming to remove these
residues.
I've got a call into Humiseal to see if they can help. Do any of you use
any other tape for masking that doesn't leave residues?
Have a great Friday!
-Steve Gregory-
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
This message (including any attachments) contains confidential and/or
proprietary information intended only for the addressee.
Any unauthorized disclosure, copying, distribution or reliance on the
contents of this information is strictly prohibited and may constitute a
violation of law. If you are not the intended recipient, please notify
the sender immediately by responding to this e-mail, and delete the
message from your system. If you have any questions about this e-mail
please notify the sender immediately.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
This message (including any attachments) contains confidential
and/or proprietary information intended only for the addressee.
Any unauthorized disclosure, copying, distribution or reliance on
the contents of this information is strictly prohibited and may
constitute a violation of law. If you are not the intended
recipient, please notify the sender immediately by responding to
this e-mail, and delete the message from your system. If you
have any questions about this e-mail please notify the sender
immediately.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
CONFIDENTIALITY NOTICE:
This e-mail, and any attachments, is for the sole use of the intended
recipient(s) and may contain information that is confidential and
protected from disclosure under the law. Any unauthorized review, use,
disclosure, or distribution is prohibited. If you are not the intended
recipient, please contact the sender by reply e-mail, and
delete/destroy
all copies of the original message and attachments.
Thank you.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|