TECHNET Archives

November 2001

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Elensky, Richard" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Wed, 7 Nov 2001 11:52:39 -0800
Content-Type:
text/plain
Parts/Attachments:
text/plain (79 lines)
Michael,

Given the size of the Minipak, it is not unreasonable to have the preheater
at such a high temp.  Preheater temperature is a function enregy emitted
(IR, convection, etc.) length of heated zone and conveyor speed.

If you profile your Mini' just as you would profile your reflow oven, you
can see if 600° F is obtaining the desired temperature on the assembly.

Have a great day.

Rich


Richard Elensky
Sr. Manufacturing Engineer
[log in to unmask] <mailto:[log in to unmask]> 

Tel:  559-292-1111  x246
Fax:  559-292-9355

Dantel
2991 North Argyle Ave.
Fresno, CA, 93727
Visit our web site at:
http:// www.dantel.com <http://www.dantel.com> 


        ----------
        From:  Michael Bell [SMTP:[log in to unmask]]
        Sent:  Wednesday, November 07, 2001 11:22 AM
        To:  [log in to unmask]
        Subject:  [TN] Electrovert Minipak 300

        Hey all,

        I anyone using an Electrovert Minipak 300 wave soldering machine???
I have
        one we use occasionally for smaller products/prototyping for various
        customers, and I am keen on finding out the average pre-heater
temperatures
        people are using.  I have only recently descovered, that ours is set
at
        around 600 degrees F.  This seems very high to me, does anyone have
any
        comments???

        Cheers

	
----------------------------------------------------------------------------
-----
        Technet Mail List provided as a free service by IPC using LISTSERV
1.8d
        To unsubscribe, send a message to [log in to unmask] with following
text in
        the BODY (NOT the subject field): SIGNOFF Technet
        To temporarily halt delivery of Technet send the following message:
SET Technet NOMAIL
        Search previous postings at: www.ipc.org > On-Line Resources &
Databases > E-mail Archives
        Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
        information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
	
----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2