TECHNET Archives

September 2000

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
Geoff Layhe <[log in to unmask]>
Date:
Tue, 26 Sep 2000 14:16:21 +0100
Content-Type:
text/plain
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Geoff Layhe <[log in to unmask]>
Parts/Attachments:
text/plain (41 lines)
Hi Frank,
Plating cracks are usually due to build up of organics in the plating bath,
maybe you need to do a carbon treat. Is this an isolated case? Is it just
one hole or a number of holes on just one board? If it's an isolated case it
may not be the plating bath.
What does the hole look like when it's sectioned? Is the hole wall rough?
Protruding fibres may lead to stress raisers. Is the electroless or direct
metalisation OK ? If this isn't continuous it can lead to "plating folds"
which can separate on thermal shock.
Hope this helps.
Sounds like you need the luck of the Irish.
Geoff
> ----------
> From:         Frank Davies[SMTP:[log in to unmask]]
> Reply To:     TechNet E-Mail Forum.;Frank Davies
> Sent:         26 September 2000 10:19
> To:   [log in to unmask]
> Subject:      [TN] Plating Cracks
>
> Just some advice if possible.  I have a board that shows a plating crack
> in the barrel and another with a plating crack at the knee (corner). The
> hole is a via .3mm with about 20 to 21 microns of plating (checked by
> micro section) This is a first this year and cannot find any cause. Could
> someone out there give me a starting point please. Thank you first.
> Frank
>

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

ATOM RSS1 RSS2