Joe Malley <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Wed, 24 Feb 1999 10:09:37 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (62 lines)
Joe G Malley@MACDERMID
02/24/99 10:09 AM
Guenter.

Is this correct expression "phase"?  I think the word may be derived from
Latin.

Joe Malley
MacDermid Inc.




Guenter Grossmann <[log in to unmask]> on 02/24/99 07:49:45 AM

Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
      to Guenter Grossmann <[log in to unmask]>

To:   [log in to unmask]
cc:    (bcc: Joe G Malley/MacDermid/MACDERMID/US)

Subject:  [TN] English expression




Hi all

Could someone give me the English expression to describe in what state (
solid, liquid, gas ) a substance is. In German we call it Aggregatszustand
( just a hint for those with German background ). Thanks a lot.

Best regards

Guenter

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2