It is quite amazing how many components have been switched to >95% tin without notification and change of part numbers. Without a disciplined parts pedigree program many contractors have expended major resources on mitigation for PMP issues. This issues are more common than most believe and additional events are uncovered against legacy safeguards for whisker prevention.
Jeffrey Bush
Sr. Principle Product Assurance Engineer
Space Products and Systems - Performance Excellence
BAE SYSTEMS
P.O. Box 868, MER24-116A
Nashua, NH 03061-0868
Facility: 144 DW Highway
Merrimack, NH 03054
Office +1 603.885.8137
Mobile +1 603.318.8056
Fax +1 603.885.5258
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Friday, November 19, 2010 10:16 AM
To: [log in to unmask]
Subject: [TN] Tin strikes again!
Morning all!
Before I post the Quiz pictures today, I got something from one of my
friends back in Tulsa that might interest you if you haven't seen it:
http://stevezeva.homestead.com/Tyco_Letter.pdf
Tin strikes again!
While we're on the subject of whiskers, here are some Inge's more
spectacular whisker images from a while back:
http://stevezeva.homestead.com/files/daniel121b.jpg
http://stevezeva.homestead.com/files/daniel131b.jpg
http://stevezeva.homestead.com/files/daniel141b.jpg
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|