Hi Gerard!
I recommend you get a copy of the following paper (although I don't think
its the one you are looking for):
"A Model For Solderability Degradation" by Dr. Chris Hunt, SMI Conference
Proceedings 1996, Volume II, Pages 650-655".
The paper does a very good job of covering the basics of intermetallic
growth in a simple manner. Good Luck.
Dave Hillman
Rockwell Collins
[log in to unmask]
[log in to unmask] on 12/29/97 02:11:06 PM
Please respond to [log in to unmask]; Please respond to
[log in to unmask]
To: [log in to unmask]
cc: (bcc: David D Hillman/CedarRapids/Collins/Rockwell)
Subject: [TN] CuSn Intermetallic growth
I seem to recall that a study was done a while back regarding the rate of
growth of Copper tin intermetallics each time a panel was subjected to the
HASL process , including reworks.
Any information on said subject?
Regards.
Gerard O'Brien.
Photocircuits Corporation
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################
|
|
|