Nice thought, but as was rehearsed endlessly in the LF forum some years ago:
this stockpiling would amount to less than 1% of the total world lead
consumption so would not result in anything much with respect to
supply/demand and therefore price. At around $0.60/kg Oklahoma would sink
under the weight before you got enough for even a small fortune, you would
also need to live a very long time.
Regards
Mike
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Hfjord
Sent: Thursday, September 21, 2006 10:21 PM
To: [log in to unmask]
Subject: Re: [TN] LF
Steve,
want be rich?
1.Begin buying all Lead that will be left when the US and others throw it
out. (Lead can't be destructed and isn't allowed to be dumped, so you will
be very welcome everywhere)
2. Wait.
3. Wait.
4. Sell your Lead when the whole world is crying for Lead again..
You'll be richest man in Oklahoma.....
Inge
----- Original Message -----
From: "Steve Gregory" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Thursday, September 21, 2006 10:45 PM
Subject: Re: [TN] LF
uhhhh...I think I'm having a déjà vu all over again...
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Dehoyos, Ramon
Sent: Thursday, September 21, 2006 3:42 PM
To: [log in to unmask]
Subject: [TN] LF
Mike Martel, a man with a positive attitude.
Ramon
Jun 26, 2006 (See Comments Below)
Editorial
Managing the Naughty Child
Mike Martel, Editor, Circuitnet
I've been listening to voices on both sides of the RoHS issue and the more I
hear, the more foreboding the tone becomes. Despite what some writers have
suggested to me, i.e., don't fight it, get with the program
- I think the electronics manufacturing industry has a real mess on its
hands that will only grow in complexity as new lead-free assemblies age in
the field. The ultimate outcome, as one friend commented the other day at
lunch, will probably be the granting of so many exemptions - necessary
ones - that the whole experiment in going lead-free will have proven to be a
many-headed hydra, a RoHarce farce that will ultimately spawn more problems
than its short-sighted authors could ever have hoped to solve. Somehow I
recall the old proverb that the Road to Hell is paved with Good Intentions.
The implications of the impending RoHS-inspired process and reliability
quagmire came to me in hints and whispers - actually, whiskers, the tin
kind - a year ago when I was looking into efforts and studies that iNEMI was
involved in regarding mitigating tin whisker growth.
Tin Whiskers. Source: Circuits Assembly Magazine Tin is a problematic,
spooky metal, and I suppose that the electronics industry would be glad to
get rid of it if only there were a suitable or economically feasible
replacement. It does strange things - such as turn to powder at very cold
temperatures, grow whiskers, etc., and while I am neither metallurgist nor
scientist in any qualification, I do understand that tin, like a naughty
child, can be governed when paired with its strict nanny, lead. Right now I
hear that the most popular tin/lead replacement alloys, SAC-alloys,
unfortunately have problems with tin whiskering, but even worse than that,
they are prone to serious voiding problems that may compromise the integrity
of the soldered connections.
One solder paste supplier, Cobar BV, appears to have addressed the voiding
problem with one specific SAC alloy. Since we recognize that voids don't
come from the alloy itself but must be related to the flux, Cobar, which has
been working for a long time in the development of high heat tolerant
synthetic fluxes, focused on the purity of the synthetic materials and
claims to have a void-free formula that is currently producing millions of
joints in consumer electronic products for a major European maker.
That being said, we still must look to the tin whisker issue. Being the
neophyte that I am, I recently queried Harvey Miller, who appears to have
(vociferously) taken up the standard of the Anti-RoHS Rebels, is the use of
conformal coating might, in some cases, particular with the tougher
coatings, prevent the growth of tin whiskers. Thinking myself a little
clever to have asked, I was nonetheless horrified to receive a response
through Harvey from a colleague of his, a Mr. John Burke:
"It is proven that conformal coating does nothing to stop tin whiskers.
It will push through the coating and will be deflected by the next coating
it comes to, so it is kind of OK in that respect unless you have a whisker
coming from the other direction. It does nothing for whiskers under the
coating, since they will propagate regardless."
Like little hypodermics, yes? I would not have expected it, so I suspect
that as whiskers grow, they grow, like an asparagus, from the base, pushing
upward and away. Harvey writes further:
"When I asked Carol Handwerker if silver could stop tin whisker formation,
she replied "only lead". (Carol Handwerker is Professor of Materials
Engineering at Purdue University, and the former chief of the Metallurgy
Division at NIST and moderator of the first iNEMI Tin Whisker Workshop). I'm
sure the process can be ameliorated one way or other but not reliably
stopped. Kirkendall voids are more insidious because copper will diffuse
into tin w/o lead, leaving voids behind. Drop your cell phone and open
circuits result. We could go on."
"The present Environmental Commissioner at the EU Parliament is Stavros
Dimas from Greece. I suspect he would like to get rid of the lead ban.
He wrote someone that he is aware of how much additional energy it will
waste because of higher temperatures. But reversing is not that easy when so
many egos and so much money have been invested in lead-free. So it will take
some time, but it will be reversed."
Now that's optimism. Let's see how it plays out.
Mike Martel, Editor
Circuitnet
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
***This email, its content and any files transmitted with it are intended solely for the addressee(s) and may be legally privileged and/or confidential. If you are not the intended recipient please delete and contact the sender by return and delete the material from any computer. Any review, retransmission, dissemination or other use of, or taking of any action in reliance upon, this information by persons or entities other than the intended recipient is prohibited.
Messages sent via this medium may be subject to delays, non-delivery and unauthorized alteration. This email has been prepared using information believed by the author to be reliable and accurate, but Indium Corporation makes no warranty as to accuracy or completeness. In particular, Indium Corporation does not accept responsibility for changes made to this email after it was sent. Any opinions or recommendations expressed herein are solely those of the author. They may be subject to change without notice.***
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|