TECHNET Archives

October 2016

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Matthias Mansfeld <[log in to unmask]>
Date:
Thu, 6 Oct 2016 08:18:16 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Message-ID:
Subject:
From:
Joyce Koo <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (36 lines)
agree with Matthias.  cure, you get skin 1st (tack free - oxidation or
surface cure), it would be hard for bubble to pop, most likely, the least
resistance place to expand - adjacent area that is not form the skin - big
bubble - bridge few sj...
> On 6 Oct 2016 at 4:59, Nigel Burtt wrote:
>
>> Are "solvent bubbles" a peculiar problem with this type of conformal
>> coating or a generic problem for coatings?
>>
>> Hypothetically if coating penetrates under the body of a low stand-off
>> component and a solvent bubble remains trapped under there after the
>> cure/dry, could that bubble "pop" under thermal cycling or high stress
>> service environment with enough force to fracture the solder joints on
>> the part?
>
> Just a guess, but I would be afraid that the solvent (which is
> assumed to be away after curing) remains for "ever" or at least long
> enough to make trouble. Remaining solvent in any traps does, what it
> is supposeed to do: solve stuff, especially if it is well trapped in
> its own bubble and has in the worst case really long time to attack
> stuff.
>
> Regards
>
> Matthias
>
> --
> Matthias Mansfeld Elektronik * Printed Circuit Board Design and
> Assembly
> Neithardtstr. 3, D-85540 Haar, GERMANY
> Phone: +49-89-4620 0937, Fax: +49-89-4620 0938
> Internet: http://www.mansfeld-elektronik.de
> OpenPGP: http://www.mansfeld-elektronik.de/gnupgkey/mansfeld.asc
> Fingerprint: 6563 057D E6B8 9105 1CE4 18D0 4056 1F54 8B59 40EF
>

ATOM RSS1 RSS2