TECHNET Archives

January 2006

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Transfer-Encoding:
quoted-printable
Sender:
Subject:
From:
Jack Crawford <[log in to unmask]>
Date:
Wed, 11 Jan 2006 16:23:26 -0600
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Jack Crawford <[log in to unmask]>
Parts/Attachments:
text/plain (37 lines)
Rick, lots of heads spinning along with yours on this requirement from your auditor. 

Of course, you would probably really put the individual in a spin to show him/her how to read the standard.  Clause 1.7.3 of J-STD-001D states:

"1.7.3 Appendices
"Appendices to this Standard are not requirements unless separately and specifically required by the applicable contracts, assembly drawing(s), documentation or purchase order."

If such documentation exists, you then got to Appendix B, Clause B-2c.  There are no "shall" words (see clause 1.5) in the appendices. Subclause c. says "Operator selected or rated temperatures of soldering systems at idle/standby SHOULD (my emphasis) be within +/- 15 º C [+/- 27 º F]. 

So unless you have other documented requirements (that would supersede the J-STD001D anyway per 1.7 and 1.7.1) and you measure BOTH ways to satisfy the auditor, there isn't any penalty if your idle temps swing more than +/- 15 º C [+/- 27 º F] because it isn't a hard requirement per J-STD-001D.

Good Luck
Jack

Jack Crawford, IOM
IPC Director Certification and Assembly Technology 
[log in to unmask] 
847-597-2893 
FAX  847-615-5693 
3000 Lakeside Drive, Suite 309 S
Bannockburn, IL, 60015

Rick Thompson wrote:

> We have a customer who is questioning how we audit soldering iron temperatures per J-STD-001D.  All of our monitoring is done in Celsius which is the main unit of measure in the standard. Imperial English (Fahrenheit) is only used as a reference shown in parentheses.  The auditor is insisting that we need to measure in both units, i.e. we have a temperature with a +/- 15C tolerance and we would also need to measure it in degrees F at +/- 27F.
<snip>

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2