Joyce, how would it affect reliability?
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Joyce Koo
Sent: Wednesday, September 11, 2013 1:18 PM
To: [log in to unmask]
Subject: Re: [TN] Gull wing solder joints and minimum electrical clearance
More likely effect your reliability than electrical clearance.
Joyce Koo
Researcher
Materials Interconnect Lab
Office: (519) 888-7465 79945
BlackBerry: (226) 220-4760
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Peter Wong
Sent: Wednesday, September 11, 2013 2:06 PM
To: [log in to unmask]
Subject: [TN] Gull wing solder joints and minimum electrical clearance
We have assemblies where gull wing solder joints have so much solder that along the side joint, the solder connection extends out to the adjacent leads similar to Figure 5-1, Image C from IPC-A-610E. "the solder connection to a termination may exhibit a wetting angle exceeding 90 degrees when it is created by the solder contour extending over the edge of the solderable termination area or solder resist" (We will be modifying our stencils to reduce the amount printed on these parts in the future).
There is no IPC-610 spec for this condition so we were thinking that if the spacing between the solder joints does not violate Minimum Electrical Clearance, they are acceptable.
Is this a correct acceptability criteria?
Thanks,
Peter
________________________________
The enclosed documents are proprietary items to Silicon Forest Electronics' (SFE) customers. They shall not be reproduced nor disclosed for any purpose except as specified in writing from an authorized agent of SFE. These documents may contain data restricted for export by the International Traffic in Arms Regulations (ITAR) section of the Arms Export Control Act (or the Export Administration Act). Violators are subject to severe criminal penalties.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|