Genny,
It is valid as far as it goes. Better test would be to sacrifice a couple of
boards and actually put them through all soldering processes as blanks and
then look for lack of wetting.
Don't forget that the intermetallic growth is heat dependent so something
that may pass one reflow cycle may not work for a double sided assembly.
If it is double sided run it through a print/reflow/print/reflow and look
for non wetting.
John
John Burke
(408) 515 4992
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Genny Gibbard
Sent: Wednesday, June 24, 2009 9:16 AM
To: [log in to unmask]
Subject: [TN] Immersion Tin solderability eval
We have some Immersion Tin boards that are several years old. From
everything I have read here or elsewhere, ImmSn is supposed to have a
short shelf life. 6 mos to a year. No one wants to scrap the boards
without testing them, though.
How would you verify whether they are still good? We hand-soldered some
pads and actually had no problems which surprised me, considering the
age of the boards, but I don't know if that is a valid test.
Genny
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|