TECHNET Archives

August 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Steve Gregory <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Steve Gregory <[log in to unmask]>
Date:
Mon, 18 Aug 2008 07:29:33 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (56 lines)
Mornin' Inge!

Got your picture posted, but that's all the help I can offer...I know
nothing about wire bonding.

Your picture is here:

http://stevezeva.homestead.com/files/Wirebond.jpg

Steve

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Hernefjord Ingemar
Sent: Monday, August 18, 2008 4:13 AM
To: [log in to unmask]
Subject: [TN] Wire bonding gurus ohoy!


 Hi all,

will send a picture to Steve for getting help.
Thermosonic 25um gold balls don't stick to the thinfilm gold on a optic
chip.
2,500A Au over 400A Cr. Bad yield, many balls lift. No contaminations
found.
Despite I have the good fishbone, I can't find out why the odd pattern
under lifted bals.
A guess is that the capillary have to steep chamfer angle, so that the
U/S mechanical energy becomes concentrated in the middle. Anyone with
similar experience?

Inge

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2