TECHNET Archives

June 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Date:
Thu, 4 Jun 1998 10:33:34 -0400
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Mike Bailey <[log in to unmask]>
Content-type:
text/plain; charset="US-ASCII"
Subject:
MIME-Version:
1.0
Content-transfer-encoding:
7BIT
Organization:
McCurdy Circuits
From:
Mike Bailey <[log in to unmask]>
Parts/Attachments:
text/plain (21 lines)
Has anyone experienced problems with packaging bare PCB's in the pink
anti-static bags?  We are seeing a "waxy"image transfer from the bag to
the panel after what appears to be several months of storage in a
controlled atmosphere.  It is aggravated by stacking individually
packaged boards on top of each other and has occurred on several
different surface finishes. The substance can also be found on the
non-board side of the bag.  Does anyone know of  what the coating might
be comprised?  Would you predict solderability issues etc?

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2