TECHNET Archives

August 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, John Burke <[log in to unmask]>
Date:
Tue, 7 Aug 2007 13:08:51 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Bev Christian <[log in to unmask]>
Subject:
From:
Bev Christian <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (214 lines)
Same here.
Bev
RIM

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of John Burke
Sent: Tuesday, August 07, 2007 12:55 PM
To: [log in to unmask]
Subject: Re: [TN] Rework question

Just looked in 7711 - didn't see a reference to it...

John

 
 
John Burke
 
(408) 515 4992

-----Original Message-----
From: Guy Ramsey [mailto:[log in to unmask]] 
Sent: Tuesday, August 07, 2007 9:14 AM
To: 'TechNet E-Mail Forum'; 'John Burke'
Subject: RE: [TN] Rework question

I don't think it is worded as a hard limit. Might be IPC-7711.  

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of John Burke
Sent: Tuesday, August 07, 2007 12:04 PM
To: [log in to unmask]
Subject: Re: [TN] Rework question

The question actually came up because there is stated (somewhere?) in an
IPC
document the number of reflow cycles you are allowed to put the board
through.

Taking that limit into account (first side reflow, second side etc)
allowed
them to remove and replace the same component 3 times in a worst case
scenario.

And I agree with Bev the whole thing is open to interpretation as to
what
represents a reflow cycle - pad dressing removal etc.


 
 
John Burke
 
(408) 515 4992
-----Original Message-----
From: Bev Christian [mailto:[log in to unmask]]
Sent: Tuesday, August 07, 2007 8:53 AM
To: TechNet E-Mail Forum; John Burke
Subject: RE: [TN] Rework question

John,
I am having people look, but if there is a limit I do not remember.
However, from a practical point of view, the answer is Doug Pauls'
patented (Or is that copyrighted or trade marked? Being a lawyer, I
don't
know.) phrase, "It all depends".  It depends on the method of rework,
(reflow, wave solder, selective soldering, soldering iron, hot air gun
focused IR, flame), temperatures reached, ramp rates, dwells, size of
board,
thickness of board, type of component, heat sinks, skill of operator. I
could go on.  Make yourself a fishbone diagram.

And then are we talking about say 3X of the same component, or 5X
side-by-side or 7x but each in a thermally separated area from the other
six?

Here's a scenario for you: double sided reflow and then required rework
under cans on both sides of the board. So this means two more for can
removal, dressing the can pads, removing the components, dressing the
pads,
part deposition, can replacement.  And hope everything works!

So you need visual inspection, x-ray inspection, electrical test and if
you
really want to do it right, x-sectioning and a whole battery of
reliability
testing.

I have seen good work and I have seen thin boards delaminated after a
single, poor attempt at rework.

Bev
RIM 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of John Burke
Sent: Tuesday, August 07, 2007 10:29 AM
To: [log in to unmask]
Subject: [TN] Rework question

Hi,

 

I had a question yesterday which was "has the number of re-work cycles
allowed by IPC changed for lead free?"

 

And I confess I don't know but I bet someone on this link does.

 

If you could let me know number of thermal cycles allowed and the spec
reference I would be grateful.

 

John

 

 

 

John Burke

 

(408) 515 4992

 


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per
day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information,
or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential
information, privileged material (including material protected by the
solicitor-client or other applicable privileges), or constitute
non-public
information. Any use of this information by anyone other than the
intended
recipient is prohibited. If you have received this transmission in
error,
please immediately reply to the sender and delete this information from
your
system. Use, dissemination, distribution, or reproduction of this
transmission by unintended recipients is not authorized and may be
unlawful.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2