TECHNET Archives

October 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Wed, 24 Oct 2007 11:22:06 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Chafin, Ken G." <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
"Chafin, Ken G." <[log in to unmask]>
Parts/Attachments:
text/plain (30 lines)
I would be interested in receiving any literature on the above subject.
Approx. 8--9 years ago we encountered many failures because  we
outsourced some surface mount boards and the supplier did a lot of
repair and replacement of SMT tantalum capacitors using soldering irons.

Both Kemet and Vishay Sprague were helpful by providing Engineering
Bulletins on the risks involved in the hand soldering of SMT tantalum
Caps.
We are again contemplating outsourcing this type of rework.  We really
need to know the risks involved in doing this and how best to do the
rework if it must be done.

Any documents (or personal experience) you think might help with this
decision would be appreciated--- [log in to unmask]

Thanks

Kenneth Chafin


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2