Hello!
Does anyone have production experiences with  Immersion Golde
over Electroless Nickel for edge connectors?
I 'm  particularly  interested in long term  Quality  and  Reliability
of contacts for  edge connector.

Thank You!

Franz  Galetsky,  UPBR.