Hi Dave, Daan and folks! I would be the first person to tell you that the
visual appearance of a solder joint does not necessarily reflect the solder
joint's integrity/reliability - that's how we got stuck with the "bright
and shiny" solder joint myth which resulted in thousands of needlessly
touched up solder connections. However, the external appearance of a solder
joint can show indications of solidification phenomena (we are dealing with
a molten metal!) - movement of a solder joint results in surface ridges
(aka a disturbed solder joint), extended/slow cool down ramps can result in
surface texture (aka grainy solder joint). The "BGA scaling" could be a
reflection of too little heat (incomplete solidification) or too much heat
(excess grain growth/structure). Either way, the reflow profile of the
assembly needs to be reviewed and corrected - unless there is some kind of
thermal issues with the assembly you should not be getting the "scaling"
effect. We have run into this on occasion and resolved the issue by
improving the reflow profile. Good Luck.
Dave Hillman
Rockwell Collins
[log in to unmask]
Daan Terstegge
<[log in to unmask] To: [log in to unmask]
> cc:
Sent by: TechNet Subject: Re: [TN] BGA
Scaling
<[log in to unmask]>
10/15/2003 02:00
PM
Please respond to
"TechNet E-Mail
Forum."; Please
respond to Daan
Terstegge
Dave's photo's can be viewed on
http://www.smtinfo.net/forum/index.php?showtopic=22
Clicking on the thumbnails gives a larger picture.
Dave, you could have posted these pics yourself, although the bmp-file
needed to be converted to a smaller jpeg to get an acceptable filesize.
B.T.W. to me this doesn't look like a bad condition, it's obvious that the
ball has fully reflowed.
Daan Terstegge
----- Original Message -----
From: "Dave Chapman" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Wednesday, October 15, 2003 8:03 PM
Subject: Re: [TN] BGA Scaling
> Daan Tertegge will be posting the pictures on www.smtinfo.net Thanks Daan
> And thanks to Sr. Ellis for the correction.
> Dave C.
>
> -----Original Message-----
> From: Dave Chapman
> Sent: Wednesday, October 15, 2003 10:57 AM
> To: [log in to unmask]; [log in to unmask]; Dave Chapman
> Cc: [log in to unmask]
> Subject: RE: [TN] BGA Scaling
>
>
> Dave I sent you a couple of pictures, I could not send through Technet.
> Dave C.
>
> -----Original Message-----
> From: [log in to unmask] [mailto:[log in to unmask]]
> Sent: Wednesday, October 15, 2003 9:48 AM
> To: [log in to unmask]; [log in to unmask]
> Cc: [log in to unmask]
> Subject: Re: [TN] BGA Scaling
>
>
>
> Hi Dave! Can you further define "BGA Scaling"? Its a term I am not
familiar
> with.
>
> Dave
>
>
> 10/14/2003 08:43
>
>
> -----Original Message-----
> From: Dave Chapman
> To: [log in to unmask]
> Subject: Re: [TN] BGA Scaling
>
> I am interested to find information on BGA scaling effect and
> solution, we saw this phenomena yesterday with a ERSA Scope
> demonstration. I have searched archives here and at SMTNET but no
> good information.
> Dave Chapman
> Circuit Service
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|