The hole must be .040" diameter or larger.
gary mccauley
-----Original Message-----
From: Edward Szpruch [mailto:[log in to unmask]]
Keep in mind two points:
.
2) The measuring equipment is limited to certain hole diameter.I do not
remember the exact figure,but you can not use it for small vias.
---------------------------------------------------------------------------------