Debbie,
There are several equipment manufacturers capable of building a conveyorized
OSP line.
Adam Pill(Germany, represented in this country by ECI), Eidshun Engineering
and FSL, to mention a few.
With respect to the pros and cons of immersion versus conveyorized,
experience has shown that the uniformity of an OSP coating is improved by
conveyorizing. Generally, the uniformity is a cosmetic thing, but important
to some. If you have a high production load, conveyorized equipment should
benefit from a productivity stand point.
Regardless, OSP coatings are thin by nature, and obviously clear in
appearance. In order to insure a cosmetically pleasing and robust
coating(necessary to prevent oxidation of the copper surface) equipment
design is very important.
Best regards,
Michael Carano
> -----Original Message-----
> From: Debbie Kenney [SMTP:[log in to unmask]]
> Sent: Friday, February 26, 1999 1:40 PM
> To: [log in to unmask]
> Subject: [TN] Entek 106A OSP
>
> Is anyone using conveyorized equipment to apply Entek 106A? If so, do you
> have the equipment suppliers name? Pros and Cons of using conveyorized
> line
> vs. tank method?
>
> Thanks in advance
>
> Debbie
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
> section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> ################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|