TECHNET Archives

July 2004

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Parial Swati <[log in to unmask]>
Date:
Fri, 16 Jul 2004 07:53:14 +0100
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Colin McVean <[log in to unmask]>
Subject:
From:
Colin McVean <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (206 lines)
Swati,

To answer in the simplest terms...

Combination of lower resin content, typically 43% and thicker glass weave,
which when placed adjacent to thick copper, say 2 oz and above can lead to
poor encapsualtion and fill capabilities. Best to go for higher resin
content prepregs when bonding thicker coppers, or attempting to fill buried
via's.

Regards,

Colin McVean

Circuit Manufacture Ltd
Unit 9-12
Rowleys Green Lane
Longford
Coventry
CV6 6AG

Tel: 02476 666168
Fax: 02476 637089
________________________________________________

This email is confidential and intended solely for the use
of the individual to whom it is addressed. Any views or
opinions presented are solely those of the author and do
not necessarily represent those of the Company.

If you are not the intended recipient, be advised that you
have received this email in error and that any use,
dissemination, forwarding, printing, or copying of this
email is strictly prohibited.

If you have received this email in error please notify the
Company by telephone on +44 (0)24 7666 6168 or reply
by email to the sender and delete the email.
________________________________________________

Whilst every effort has been made to ensure that there are
no viruses embedded in this email, we highly recommend
that you virus scan any attached files using your own anti-
virus software.


-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Parial Swati
Sent: 16 July 2004 04:41
To: [log in to unmask]
Subject: Re: [TN] 7628 prepreg?


Why is it that laminate voids are likely with such a combination ?

Regards,
Swati...


|---------+---------------------------->
|         |           Eddie Rocha      |
|         |           <[log in to unmask]
|         |           M>               |
|         |           Sent by: TechNet |
|         |           <[log in to unmask]>|
|         |                            |
|         |                            |
|         |           07/15/2004 10:29 |
|         |           PM               |
|         |           Please respond to|
|         |           "TechNet E-Mail  |
|         |           Forum."; Please  |
|         |           respond to Eddie |
|         |           Rocha            |
|         |                            |
|---------+---------------------------->

>---------------------------------------------------------------------------
-----------------------------------|
  |
|
  |       To:       [log in to unmask]
|
  |       cc:       (bcc: Parial Swati/NAN/ATS/IN)
|
  |       Subject:  Re: [TN] 7628 prepreg?
|

>---------------------------------------------------------------------------
-----------------------------------|




7628 aginst 2 oz copper is not recommended. Possible lamination issues are
likely, i.e. lam voids.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Brooks,Bill
Sent: Tuesday, July 13, 2004 9:46 AM
To: [log in to unmask]
Subject: Re: [TN] 7628 prepreg?


So in a stackup that requires a .031 core with 2 oz. Cu both sides and a
symmetrical build up of 2 layers of 7628 on both sides (4 total) and then
1.5 oz Cu finished outside... Would the objective then be to control the
spacing from the outer conductors to the inner ground plane at .014 in.?

Is the DK of 7628 different than other glass epoxy materials? I would like
to calculate the impedance of the traces on this board.

Is there a materials sheet available on-line that describes the electrical
and physical characteristics of the prepreg material? And does it change
when laminated?

This is an older board and I'm just trying to decipher the designer's
intent.

Thanks in advance...

Bill Brooks
PCB Design Engineer , C.I.D., C.I.I.
Tel: (760)597-1500 Ext 3772 Fax: (760)597-1510
http://pcbwizards.com

-----Original Message-----
From: Jeffrey Bush [mailto:[log in to unmask]]
Sent: Tuesday, July 13, 2004 4:10 AM
To: [log in to unmask]
Subject: Re: [TN] 7628 prepreg?

7628 glass has different yield thickness based on resin content and the
rheology.  You can purchase 7628 in epoxy from a yield per ply thickness
of .0065" to where you are with yours.  7629 glass can give you up to
.009" in yield as this is some what heavier glass.  I think the standard
has been a .007" per ply yield - this is fairly standard from laminate
suppliers.



Jeffrey Bush
Director, Quality Assurance and Technical Support

                          76 Technology Drive - POB 1890
                             Brattleboro, Vermont 05302-1890
                                Tel. 802.257.4571.21 Fax. 802.257.0011
                                    [log in to unmask]
                              http://www.vtcircuits.com

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------



Scan by AT&S virus protection

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2