Try it this way:
http://www.bobwillis.co.uk/guide/cracking%20chip%20capacitors.pdf
Just an odd thought - could your cracking issue be MSD caused? We have
seen some ceramic bodied parts marked at a much higher moisture
sensitivity level then expected and had issues with them cracking in
reflow. The result looked like delamination of the layers.
Jeffrey A McGlaughlin, CID
Engineering Designer
Battelle
505 King Ave
Columbus Ohio 43201-2693
Phone (614)424-7582
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Igoshev, Vladimir
Sent: Tuesday, July 15, 2008 9:19 AM
To: [log in to unmask]
Subject: Re: [TN] Ceramic caps
And that is exactly what I did. There are two spaces in the link
(between the words cracking chip capacitors) which are not supposed to
be there.
www.bobwillis.co.uk/guide/cracking chip capacitors.pdf
Regards,
Vladimir
-----Original Message-----
From: Rex Waygood [mailto:[log in to unmask]]
Sent: Tuesday, July 15, 2008 9:16 AM
To: TechNet E-Mail Forum; Igoshev, Vladimir
Subject: RE: [TN] Ceramic caps
Yes it does, but you need to cut and paste all of it into your browser
[log in to unmask]
www.PartnerTech.co.uk
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Igoshev, Vladimir
Sent: 15 July 2008 14:06
To: [log in to unmask]
Subject: Re: [TN] Ceramic caps
Hi Bob,
The link doesn't work.
Regards,
Vladimir
-----Original Message-----
From: Bob Willis [mailto:[log in to unmask]]
Sent: Tuesday, July 15, 2008 2:25 AM
To: 'TechNet E-Mail Forum'; Igoshev, Vladimir
Subject: RE: [TN] Ceramic caps
The following text outlines many of the common and less common reasons
for cracking capacitors. The problem is less common today but has always
been a issue in industry.
www.bobwillis.co.uk/guide/cracking chip capacitors.pdf
Many thanks
Bob Willis
2 Fourth Ave, Chelmsford, Essex, CM1 4HA England
Tel: (44) 1245 351502
Fax: (44) 1245 496123
Mobile: 07860 775858
www.ASKbobwillis.com
New Bob Willis "Printed Board Inspection & Quality Control Workshop" 3rd
September www.ASKbobwillis.com/PCBworkshop.pdf
Book your place on Bob's "Step by Step Failure Analysis Workshop" 11th
September www.ASKbobwillis.com/faworkshops.pdf
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Igoshev, Vladimir
Sent: 14 July 2008 14:08
To: [log in to unmask]
Subject: [TN] Ceramic caps
Hi TechNeters,
I came across an unusual (at least to me) failure mode of ceramic caps.
They crack along the component body in either normal (from top all the
way through to the bottom), or parallel (from one side all the way
through to the other side) direction to the board the caps are mounted
on.
Has anyone seen something similar?
Thanks a lot in advance.
Regards,
Vladimir
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
------------------------------------------------------------------------
-------
The information contained within this e-mail and any attachments
contained therein may be confidential and/or legally privileged and is
for the use of the intended recipient only. If you are not the intended
recipient please delete it from your system and notify the sender by
return e-mail. The content of this e-mail may not be copied or disclosed
to any third parties without prior permission from the sender.
E-mail is susceptible to data corruption, interception, tampering and
viruses. We do not accept any liability for any such incidents or any
consequences thereof.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|