TECHNET Archives

March 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Wed, 23 Mar 2005 09:26:13 -0000
Reply-To:
Subject:
From:
Mike Fenner <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (286 lines)
Late again...
I just have a little query for the more informed than me: 
I have vague memories about MIL 883, plating integrity, corrosion testing,
salt spray and stuff like that. 
This be OK?

Regards

Mike 




-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Creswick, Steven
Sent: Friday, March 18, 2005 8:41 PM
To: [log in to unmask]
Subject: Re: [TN] Solder on top of LCCC


Steve - If truely a metal to metal weld, and not soldered, then I will also
agree that this may only be a cosmetic issue.  

We also used seam welders to reflow solder Au-Sn 'combo lids', so the use of
this equipment [alone] does not necessarily mean it is welded.  Your
supplier should know his process, but I like Bill's suggestion.

We used to de-lid reflowed lids by sliding a single edge razor blade between
the lid and the package seal surface.  If you can not do this easily - it is
likely welded.  Good news!

Steve

-----Original Message-----
From: Bill Kasprzak [mailto:[log in to unmask]]
Sent: Friday, March 18, 2005 2:13 PM
To: [log in to unmask]
Subject: Re: [TN] Solder on top of LCCC


Steve,

You've got the answers to your question.

Is this vendor willing to put the answer in writing?  If so, you are in
great shape.

Too often I've found vendors willing to bend but unwilling to put it
writing. In the age of suing everyone, who could blame them.

Bill Kasprzak
Moog Inc
Process Engineer, Electronic Assembly



Stephen Gregory <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
03/18/2005 01:56 PM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
[log in to unmask]


To
[log in to unmask]
cc

Subject
Re: [TN] Solder on top of LCCC






Hi Steve,

These are for a class-3 military application. This is a oscillator
M55310/19-BO3A40000
made by XSIS Electronics (they're out my way in Shawnee, Kansas).

I called them and they said they should be fine. The lid is welded with a
seam sealer and
there is no solder used, is what I was told.

-Steve Gregory-



|---------+---------------------------->
|         |           "Creswick,       |
|         |           Steven"          |
|         |           <SCreswick@GENTEX|
|         |           .COM>            |
|         |           Sent by: TechNet |
|         |           <[log in to unmask]>|
|         |                            |
|         |                            |
|         |           03/18/2005 10:13 |
|         |           AM               |
|         |           Please respond to|
|         |           TechNet E-Mail   |
|         |           Forum; Please    |
|         |           respond to       |
|         |           "Creswick,       |
|         |           Steven"          |
|         |                            |
|---------+---------------------------->

>---------------------------------------------------------------------------
-----------------------------------|
  |                                       |
  |       To:       [log in to unmask]  |
  |       cc:                                       |
  |       Subject:  Re: [TN] Solder on top of LCCC                |

>---------------------------------------------------------------------------
-----------------------------------|




Steve,

I would add a degree of caution here.  Many of the good ol' high temp
co-fired LCC's used gold-tin [80/20] for sealing of the lid to the
package.

If you immerse the gold-tin into normal tin bearing solder, eventually
your
package seal will be compromised.

I would lean to the side of WHAT your QA people are saying, but not
BECAUSE
of what they are saying and reject these units.   .... but then I do not
know what the application is either ...  Likely not to use them in Mil
product

Just my two bits

Steve C

-----Original Message-----
From: Stephen Gregory [mailto:[log in to unmask]]
Sent: Friday, March 18, 2005 10:46 AM
To: [log in to unmask]
Subject: [TN] Solder on top of LCCC


Happy Friday All Ya'll!!

We have some LCCC's that needed gold removal, and we did them here
in house manually. The lady that I had doing this was really careful, but
she
got some solder on top of a few of them.

QA was wanting to scrap them because of "solder contamination". I disagree
that they should be scrapped. I can't find any spec that says they need to
be
scrapped. You can still read the part numbers, and there are no solder
shorts
from the castellations to the top. Go to:

http://www.stevezeva.homestead.com

and look at "Solder on LCCC", and tell me what you think....these are
$50.00 ea.
and I don't want to scrap them if I don't have to.

Kind regards,

-Steve Gregory-
Senior Process Engineer
LaBarge Incorporated
Tulsa, Oklahoma
(918) 459-2285
(918) 459-2350 FAX
__________________________________________________________________
This message may contain information that is privileged and confidential
to
LaBarge, Inc.  It is for use only by the individual or entity named above.
If you are not the intended recipient, you may not copy, use or deliver
this message to anyone.  In such event, you should destroy the message and
kindly notify the sender by reply e-mail.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------



__________________________________________________________________
This message may contain information that is privileged and confidential
to
LaBarge, Inc.  It is for use only by the individual or entity named above.
If you are not the intended recipient, you may not copy, use or deliver
this message to anyone.  In such event, you should destroy the message and
kindly notify the sender by reply e-mail.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------


:::::::::::::::::::::::::::

This email, its content and any files transmitted with it are intended solely for the addressee(s) and may be legally privileged and/or confidential. If you are not the intended recipient please delete and contact the sender by return and delete the material from any computer. Any review, retransmission, dissemination or other use of, or taking of any action in reliance upon, this information by persons or entities other than the intended recipient is prohibited.

Messages sent via this medium may be subject to delays, non-delivery and unauthorized alteration. This email has been prepared using information believed by the author to be reliable and accurate, but Indium Corporation makes no warranty as to accuracy or completeness. In particular, Indium Corporation does not accept responsibility for changes made to this email after it was sent. Any opinions or recommendations expressed herein are solely those of the author. They may be subject to change without notice.

:::::::::::::::::::::::::::

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2