The old SnPb solder fractures!!!!
Victor,
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Chris Mahanna
Sent: Wednesday, August 06, 2014 1:48 PM
To: [log in to unmask]
Subject: [TN] SJ fracture signature
We see hundreds of cracked solder joints every year, but I can't say that I've ever seen one quite like this. I have some suspicions, but I'll keep them to myself, as to not prejudice the crowd.
EDS maps are forthcoming.
This is a caught in-the-wild field failure of a 48-pin BGA Reballed to SnPb ENIG on board side Ni barrier on component side
http://stevezeva.homestead.com/45268-1.JPGhttp://stevezeva.homestead.com/45268-2.JPGhttp://stevezeva.homestead.com/45268-8.JPG
Thoughts? And Thanks to Steve!
Chris Mahanna
President, Technical Manager
Robisan Laboratory Inc.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________