Hi,
We are using nitric acid for stripping of plating racks and during this
process some amount of NOx escapes to air.
We have been requested by environmental authorities to install wet scrubber
for absorption of NOx.It seems,that diluted alkaline solution ( such as
caustic soda ) will do the job of absorption of NOx.
What is the common practice? I presume some of plating shops are using
nitric acid for racks stripping.
Best regards
Edward
Edward Szpruch
Eltek , Manager of Process Engineering
P.O.Box 159 ; 49101 Petah Tikva Israel
Tel ++972 3 9395050 , Fax ++972 3 9309581
e-mail [log in to unmask]
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|