TECHNET Archives

February 2005

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Dennis Fritz <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Tue, 1 Feb 2005 09:57:29 EST
Content-Type:
text/plain
Parts/Attachments:
text/plain (29 lines)
In a message dated 2/1/2005 9:35:26 AM Eastern Standard Time,
[log in to unmask] writes:

Last  year we tried to plate copper through holes on LCP.   Blistered
everywhere, top surface, in holes.


LCP is interesting resin.  To plate electroless copper  with adhesion, it
needs a special adhesion promotion treatment - a lot different  from epoxy glass.
I agree, if you just run it down a regular electroless copper  line, you will
get the worst hole wall pull away you have ever seen.

Contact me off line for a copy of the cycle that MacDermid  recommends for
plating the shielding on LCP connector bodies.  The same  cycle works on LCP
core laminate, and I think would work on molded interconnect  devices.

Denny Fritz
MacDermid

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2