Hi, In my past I seen similar results caused by lack of current to specific
boards, or areas caused by oxidized buss bars or improper connectivity on
the board them selves. Sometime just cleaning your buss bars on a daily
basis will prevent the majority of your problems. Check with a simple
continuity meter circuits on boards to see if there are any opens. Best of
Luck Jim Jablonsky
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Anan
Sent: Thursday, September 01, 2005 12:10 PM
To: [log in to unmask]
Subject: Re: [TN] chocolate plating
Hi :
the amazing that not all the board have this chocolate copper , some times
maybe just little area in the board have the chocolate cooper and the other
areas in the board OK ,also not all the panels in the batch that was in the
tank have a chocolate copper .
the hull-cells is OK .
the anode film look OK
Zreik Anan
Technology Manager PCB
P.O.B 631 Migdal Haemek 23105
Tel : 972-46544300 Ext -267
Mobile : 972-577675569
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Dennis Fritz
Sent: Thursday, September 01, 2005 5:10 PM
To: [log in to unmask]
Subject: Re: [TN] chocolate plating
Good suggestion from George Milad. Copper plates well to copper, but not
well to copper oxide. Is this chocolate all over the boards, or in
patches?
You may want to check for impurities now in the bath. Organics usually
show
on hull cells - have you run that on the bath?
Inorganic contaminants cause the following problems (From IPC 740 trouble
shooting guide, chapter 10)
What does the anode film look like - may be a way a clue to what is
happening on the boards?
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|