Hi Vladimir,
What you said is true for most X-ray equipment—and it is also true in
practical terms. however, you can see solder joint fractures with X-ray if you focus
on a single solder joint [not very practical] and look at it by rotating this
SJ.
I have a QuickTime movie showing it.
Werner
**************
The year's hottest artists on the red carpet at the Grammy
Awards. Go to AOL Music.
(http://music.aol.com/grammys?NCID=aolcmp00300000002565)
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------