No one uses 8 mil traces anymore, especially on a design like that.
You gotta get two traces between pins....
(just one lowly designer's opinion)
Jack
-----Original Message-----
From: John Parsons [mailto:[log in to unmask]]
Sent: Friday, December 17, 1999 11:06 AM
Subject: Need Design Advice for BGA (?) Socket
Seasons Greetings!
We have just received a design from a customer which
utilizes a
560 pin BGA(?) socket. Here are the details;
-6 Layer board, 4 routing layers 2 plane layers
-Socket is 5 rows deep
-Current configuration - 23mil hole on 30mil pad on 50mil
grid
-Routing out with 8mil traces on primary, secondary and two
inner
layers
We have told him that his hole to pad ratio is too small for
us to
manufacture. Currently our minimum spec is 6mil annular
ring (pad
dia - finished hole size/2) for outer layers and 7.5mil for
inners
(although we will do 6mil on inners if we have to).
He is telling us that he cannot design within these
constraints.
What are others doing for this design? Are you routing out
on
outer layers? We cannot seem to put our hands on another
sample design from our files (although I know they are some
in
there somewhere).
Regards
John Parsons
Circuit Graphics Ltd.
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|