TECHNET Archives

March 2014

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Fri, 21 Mar 2014 13:21:21 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Stewart McCracken <[log in to unmask]>
Subject:
MIME-Version:
1.0
Message-ID:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="utf-8"
From:
Stewart McCracken <[log in to unmask]>
Parts/Attachments:
text/plain (88 lines)
Hi Steve,

Please add MCS to your list - please see www.themcsgroup.co.uk
We have lots of experience with wire bond analysis. 

Thanks

Stewart

Stewart McCracken
MCS Ltd.
07711 541735

---- Vladimir Igoshev wrote ----

Hi Steve,

You can add our lab to that list.

Regards,

Vladimir Igoshev
SENTEC Testing Laboratory Inc.
11 Canadian Road, Unit 7
Scarborough, ON M1R 5G1
Phone: 647-495-8727
Cell: 416-899-1882
[log in to unmask]
www.sentec.ca
  Original Message  
From: Steven Creswick
Sent: Friday, March 21, 2014 8:37 AM
To: [log in to unmask]
Reply To: TechNet E-Mail Forum
Subject: [TN] Failure Analysis Labs for Heavy Wire Bonding Issues

Good morning everyone!

Hoping someone can help on this somewhat unique situation - 

A party is performing heavy wire Al bonding of 12 & 20 mil wire between a
PWB and the leads of an over-molded package. 

They are looking for an outside lab to perform testing/failure analysis in
an attempt to determine the root cause/s of frequent bond misses. (It
appears they have minimal analysis capability in-house.)

The first things that I think of with heavy wire Al bonding issues are
insufficient clamping during bonding, mold flash on the leads, mold release
on the leads, and lead oscillation (harmonics) during bonding.

Does anyone know of a good failure analysis lab that can provide these
services? The company is located in the central US, but ultimately, the lab
can be anywhere.

Two possible that come to mind are:

Foresite Labs - http://www.residues.com/

Constellation Technology, in Largo, Florida - http://www.contech.com/

Anyone have others??


Steve Creswick
Sr Associate - Balanced Enterprise Solutions
http://www.linkedin.com/in/stevencreswick
616 834 1883




______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2