TECHNET Archives

March 2011

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Mike Buetow <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Mike Buetow <[log in to unmask]>
Date:
Wed, 2 Mar 2011 09:41:46 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (106 lines)
Well, for starters, the dip paste used to stack the packages is more
prone to solder balling. This is because it has a lower metal content
and smaller solder particle than screen-printable pastes. Also, it's
fairly easy to drown the part in flux. You need to take care to apply
liquid flux only to the surface of the balls. 

I should add that Bob Willis is doing a webinar on PoP during Virtual
PCB next week. 
http://circuitsassembly.com/cms/news/10851-pop-signal-integrity-webinars
-highlight-virtual-pcb


Best,
Mike

Mike Buetow
Circuits Assembly
w/m 617-327-4702

>>> VIRTUAL PCB, the industry's only online tech conference and
exhibition, March 8-9, www.virtual-pcb.com <<<

Follow me on Twitter: twitter.com/mikebuetow


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Christopher Young
Sent: Wednesday, March 02, 2011 9:33 AM
To: [log in to unmask]
Subject: [TN] POP THE QUESTION??

Can anyone out there give me the pitfalls of POP placement Technology
(Package on package) within manufacturing. 

 

Also names of CEM's within the UK capable of successfully placing down
such devices.

 

Regards

 

Chris

 

 


The information contained within this e-mail and any files attached to
this e-mail is private and in addition may include commercially
sensitive information. The contents of this e-mail are for the intended
recipient only and therefore if you wish to disclose the information
contained within this e-mail or attached files, please contact the
sender prior to any such disclosure. 

If you are not the intended recipient, any disclosure, copying or
distribution is 
prohibited. Please also contact the sender and inform them of the error
and delete the e-mail, including any attached files from your system. 

Cassidian Limited, Registered Office : Quadrant House, Celtic Springs,
Coedkernew, Newport, NP10 8FZ Company No: 04191036
http://www.cassidian.com

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2