TECHNET Archives

October 2002

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Fri, 25 Oct 2002 15:29:38 -0500
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Content-type:
text/plain; charset=iso-8859-1
Subject:
MIME-Version:
1.0
Content-transfer-encoding:
quoted-printable
From:
Parts/Attachments:
text/plain (88 lines)
Good catch Mel.  Obviously the meaning changes with geographic location.
Now, keep in mind I was talking about DIET Mt. Dew.  Have the good old boys
back in the 'bama hills come up with Diet moonshine yet?

With all the corn we have here, we do a lot of brewing, but it's the state
sponsored kind that goes into gasoline.  And I do know they frown on match
flicking at THOSE locations.

Doug Pauls
Advanced Operations Engineering
Rockwell Collins


                                                                                                                                       
                      Mel Parrish                                                                                                      
                      <mparrish@SOLDERI        To:       [log in to unmask]                                                               
                      NGTECH.COM>              cc:                                                                                     
                      Sent by: TechNet         Subject:  Re: [TN] Quality                                                              
                      <[log in to unmask]>                                                                                                
                                                                                                                                       
                                                                                                                                       
                      10/25/02 11:40 AM                                                                                                
                      Please respond to                                                                                                
                      "TechNet E-Mail                                                                                                  
                      Forum."; Please                                                                                                  
                      respond to Mel                                                                                                   
                      Parrish                                                                                                          
                                                                                                                                       
                                                                                                                                       





Wouldn't recommend throwing any matches at Mountain Dew from this neck of
the woods.
Course they don't do (pun intended) that in  Iowa - or do they?


Mel Parrish

-----Original Message-----
From: TechNet  [mailto:[log in to unmask]]On Behalf Of Brian Toleno
Sent:  Friday, October 25, 2002 11:01 AM
To:  [log in to unmask]
Subject: Re: [TN]  Quality



I would agree  with Rudy's comment (having experience with an FA lab in the
past).  The  best is to send, at minimum, a "known good" and a suspect,
blind the samples  and let the laboratory earn their fee.

BTW Doug, enjoyed the posting on the cleanliness, be sure to let us  know
how many matches it takes to ignite Mountain Dew.

Brian J. Toleno,  Ph.D.
Sr. Applications Chemist
Loctite Electronics
15051 East Don  Julian Rd
Industry, CA 91746
Ph: 626-968-6511 x304
Cell:  626-390-9562
--------------------------------------------------- Technet  Mail List
provided as a free service by IPC using LISTSERV 1.8e To  unsubscribe, send
a message to [log in to unmask] with following text in the  BODY (NOT the
subject field): SIGNOFF Technet To temporarily halt or  (re-start) delivery
of Technet send e-mail to [log in to unmask]: SET Technet  NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail  to
[log in to unmask]: SET Technet Digest Search the archives of previous posts
at: http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/html/forum.htm for additional information, or contact
Keach  Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------



---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2