I have seen bridges under BGAs due to solder creeping up with the solder wave. I
think that QA has a valid concern. A quick fix is kapton tape under the BGA. A
permament fix is plugged vias under the BGA.
Regards,
Arturo
Miguel Vallejo <[log in to unmask]> on 10/13/2000 12:10:17 PM
Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond to
Miguel Vallejo <[log in to unmask]>
To: [log in to unmask]
cc: (bcc: Arturo Urias/AUS/NIC)
Subject: [TN] Plated vias under BGA-mask prior to wave?
Hi,
I'm mounting a 388 package, .050 pith (AMD) BGA onto a .062 board full of
plated vias (.010 dia) throughout the BGA perimeters. Here're my questions:
Should I be concern that solder can flow up during wave solder and cause
shorts on the BGA?
If the BGA locations receives a socket, rather than the BGA, would it make a
difference?
I personally, don't think I have to mask the vias, but QA is concern.
Thank you in advance for any help.
Miguel V.
---------------------------------------------------------------------------------
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF TECHNET
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF TECHNET
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|