Jacob Ransborg wrote:
>
> Hi Technetters
>
> Thanks for the good discusion about electroless Ni/Au.
>
> I have a simple question!
> Are there someone who knows where I can material about the chemical reactions that occurs in the electroless nickel bath. We are running a bath with the components Ni, Hypo-phosphit, Ammonia and a lead stabilizer.
>
> Regards
> Jacob Ransborg
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
> For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
> ################################################################
Hi Jacob
There is a book called "electroless nickel plating".
Author: Wolfgang Riedel.Published by ASM international finishing
publications LTD.
Regards
Peter Fogelqvist
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|