TECHNET Archives

November 2016

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Yehuda Weisz <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Yehuda Weisz <[log in to unmask]>
Date:
Mon, 14 Nov 2016 23:50:42 +0200
Content-Type:
text/plain
Parts/Attachments:
text/plain (55 lines)
Thanks for the example Victor,
This is just one of those things that concern me while referring to this
parameter.
Is there a chance that you remember what was the clearance in THAT failed
board?

Best regards,
Yehuda

-----Original Message-----
From: [log in to unmask] [mailto:[log in to unmask]] 
Sent: Monday, November 14, 2016 3:30 PM
To: [log in to unmask]; [log in to unmask]
Subject: RE: [TN] Copper to edge distance

Food for thought,

   I have seen Field Return PWB in which a short was created between the PWB
edge and the metal chassis /metal hardware.   Due to spacing clearance and
solder mask thickness

Victor,

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Yehuda Weisz
Sent: Sunday, November 13, 2016 4:15 PM
To: [log in to unmask]
Subject: [TN] Copper to edge distance

Hello  Technetters,
For the beginning of the week I have a question to you that occupies me more
and more lately, and it concerns one of the design guidelines - "distance of
copper to edge".

IPC-2221 specifies the minimum distance by design as 20 mils and raises this
value as the voltage drop increases.
Well, as PCBs become more and more dense, it becomes a very challenging task
to convince designers to give up real-estate along the edges of the board.
Their claim - if the manufacturer can work with a tolerance of +/-0.1mm, why
do I need to keep a clearance of 0.5 mm along the edges.
Most of the boards we are dealing with are for high reliability customers
(class 2, class 3 type guys) and from what I have heard from other designers
- no one goes below 20 mil. Some even keep a minimum of 40 mil along the
edges.

So - my question to you is simply - WHY ???
Why did the spec. call for 20 mil minimum clearance??
I do give reasons to the designers, involving reliability and so on but I
feel that I might be missing the real point (or the fundamental reason).

Could any/some of you, knowledgeable people, help me out on this??