Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0vkyBF-0000d9C; Thu, 16 Jan 97 14:12 CST |
Encoding: |
44 Text |
Old-Return-Path: |
|
Date: |
Thu, 16 Jan 97 13:13:25 cst |
Precedence: |
list |
Resent-From: |
|
Cc: |
|
X-Status: |
|
Status: |
O |
X-Mailing-List: |
|
From [log in to unmask] Thu Jan 16 15: |
13:43 1997 |
TO: |
|
Return-Path: |
<TechNet-request> |
Resent-Message-ID: |
<"VghuY3.0.QNN.vketo"@ipc> |
Subject: |
|
From: |
|
X-Loop: |
|
Resent-Sender: |
|
Message-Id: |
|
Parts/Attachments: |
|
|
Hi TechNet!
Are the solder skips location dependent or always near specific types
of other components on the assembly? You may be getting shadowing ( an
alteration of the solder wave flow) of your components from other
components or structures on the assembly. You could also try checking
your nitrogen environment - a "cleaner" nitrogen blanket (i.e. less oxygen
ppm levels) will lower the solder surface tension and allow for additional
wetting. Note - really low surface tension can give you defects too!
Dave Hillman
Rockwell Collins
[log in to unmask]
______________________________ Reply Separator _________________________________
Subject: Assy: Solder Skip
Author: [log in to unmask] at ccmgw1
Date: 1/16/97 9:59 AM
Hi Technetters,
I am wandering anyone could suggest ways to get rid of solder skips.
We have a lot of solder skip on the Tant capacitor, case size type A
and B, but don't have any problem with the rest of the chip components
and SOICs. The pad size for the Tant Cap id pretty small, only allow
very little for space for the chip wave to be able to solder to the
terminations.
Any ideas how to fix it..We are running no-clean using a full-blow nitrogen
tunnel wave-solder machine.
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|