TECHNET Archives

October 2005

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Werner Engelmaier <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Sun, 30 Oct 2005 13:46:13 EST
Content-Type:
text/plain
Parts/Attachments:
text/plain (20 lines)
Hi Ingemar,
I have to say I have not heard the terminology 'time to obtain maximum
wetting' before, and as you point out it makes no sense. there is no such thing as
'maximum wetting'--either you are properly wetted, giving you a solid layer of
IMC(s) and thus a good metallurgical bond, or you are inadequately wetted with
little or no IMC layers and thus no metallurgical bond. Just jhaving 'nice'
looking SJs is no proof of their quality.

Werner

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2