The silver bath needs to be maintained well to avoid issues in keeping
the bath running. When the bath is not maintained do to lack of
production the bath does go south and is expensive to replenish and/or
make up a new one. We find that the bath need to be monitored for
certain components and when controlled, provides a finish that is good
for at least 1 year, if not more. Any boards that are stocked are vac
packed, which helps in shelf life. ENIG is by far the most costly
alternative, with silver close to HASL, and Tin sometimes lower cost.
Poor line setup, control support and production will maybe the cause of
you fab houses feedback on silver.
Jeffrey Bush
Director, Quality Assurance and Technical Support
VERMONT CIRCUITS INCORPORATED
76 Technology Drive - POB 1890
Brattleboro, Vermont 05302
Voice: 802.257.4571.21 Fax: 802.257.0011
http://www.vtcircuits.com
-----Original Message-----
From: Scott Lefebvre [mailto:[log in to unmask]]
Sent: Wednesday, November 24, 2004 1:43 PM
To: [log in to unmask]
Subject: [TN] Immersion Silver
I just got off the phone with one of our PCB FAB shops and was surprised
on his response to Immersion Silver as a solder finish.
He suggested that we do not use it as a replacement for HASL and to use
gold instead. All the things I've read and did research on IAg in
contraction to he said. The shop said shelf life is less than 6 months
and tarnish was a big issue. It was more expensive than ENIG and not
that many shops do it in-house.
My understanding is the shelf life is 6-12 months if stored and handled
properly. They silver used today has an anti-tarnishing agents to
prevent tarnishing. I was also under the impression that IAg is less
costly than ENIG.
Your opinion in this matter would be greatly appreciated.
Thank you,
Scott
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|