Hi,
I'm wondering if there is a published change history for IPC-A-610?
Specifically, I'm interested in the changes from Rev B to Rev C. I have an
assembly manufactured 3.5 years ago that has now failed. Upon inspection of
the workmanship, there are numerous defect conditions present. Prior to
going after the manufacturer, I would like to verify the workmanship
standards to which the product should have been built to originally.
Thanks
Marty Brooks
Manufacturing Engineer
IDENTEC Solutions, Inc.
102, 1860 Dayton Street
Kelowna, B.C., Canada V1Y 7W6
Ph:(250)860-6567, Fax:(250)860-6541
www.identec.com
This email contains confidential information and is intended for the sole
use of the addressee. Any other distribution, copying or disclosure is
strictly prohibited. If you are not the addressee, please notify the sender
by email and delete this message.
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|