TECHNET Archives

March 2013

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, lee Hitchens <[log in to unmask]>
Date:
Tue, 26 Mar 2013 13:36:05 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
From:
Douglas Pauls <[log in to unmask]>
Message-ID:
In-Reply-To:
<00d601ce2a40$8653de80$92fb9b80$@[log in to unmask]>
Content-Type:
text/plain; charset="US-ASCII"
MIME-Version:
1.0
Parts/Attachments:
text/plain (147 lines)
Lee,
I don't think you can assume that the cleaning process drying section is 
adequate.  In many cases, you may have heated air knives blowing away the 
water.  If you have highly figured assemblies (thick, dense) and low 
standoff parts, you cannot assume you got all the water out.  Many of your 
coatings don't like water when they are applied as a liquid coating, or 
while they cure.

Doug Pauls



From:   lee Hitchens <[log in to unmask]>
To:     <[log in to unmask]>
Date:   03/26/2013 11:40 AM
Subject:        Re: [TN] Conformal Coat and Board Edges
Sent by:        TechNet <[log in to unmask]>



Can I also ask a question. What is the purpose of baking a PCB before
coating, assuming that the cleaning process drying section is adequate? I
have never really got a good answer to this?

Best Regards

Lee Hitchens
Technical Director

SCH Technologies is a Division of SCH Services Limited
Mob: +44 (0) 7862 25 33 21 www.conformalcoating.co.uk

TECHNICAL SUPPORT SERVICE
 
SCH Services Ltd offers a Technical Support Helpline to help address all
issues relating to reliability. This includes contamination testing,
cleanliness and cleaning issues, plus any coating related questions.
Please contact us via email or telephone:
 
[log in to unmask]   +44 (0)1226 249019 (office hours & answerphone)   
+44
(0)7862 253321 (out-of-hours emergency)

The opinions expressed in this e-mail are strictly those of the sender and
not of SCH Services Limited. This communication may contain information
which is confidential and may also be privileged. It is for the exclusive
use of the intended recipient(s). Unauthorised use, copying or disclosure 
of
any of it may be unlawful. If you are not the intended recipient(s) please
note that any distribution, copying or use of this communication or the
information in it is strictly prohibited. If you have received this
communication in error please notify us by e-mail or by telephone (+44
(0)1226 249019) and then delete the e-mail and any copies of it. Virus
Warning - Although steps have been taken to ensure that all email and
attachments are virus-free, we cannot guarantee nor be held liable.
 
Company Registration: 04043334
Registered office: SCH Services Limited Newburgh Building McLintock Way
Barnsley South Yorkshire S70 6BF



-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Fox, Ian
Sent: 26 March 2013 16:17
To: [log in to unmask]
Subject: Re: [TN] Conformal Coat and Board Edges

No we don't. Since the purpose of the coating is not to prevent moisture
ingress into the board (we all know that happens), but really to prevent
issues with condensation, and since there likely will be no exposed tracks
on the edge, there's no point. We typically have a ground/thermal strip
around the edge of the card anyway so the masking may sometimes cover, or
partially cover the edge. I couldn't tell you how many millions of on wing
hours our assemblies have accumulated over the past 30+ years, but we've
never had an issue in service as a result of uncoated edges, nor in the
umpteen unit qualifications we've carried out. In fact if you carry out
weight gain measurements with high (85%+) humidity exposure the laminate 
is
typically saturated after about 4 days and we always run the 10 day 
tropical
exposure test

Regards

Ian Fox
Lead Materials and process Engineer
 
Aero Engine Controls
York Road, Hall Green, Birmingham B28 8LN | Tel: +44 (0)121 607 3763 | 
Fax:
+44 (0)121 607 3975
Email: [log in to unmask] | Web: www.aeroenginecontrols.com
 
Aero Engine Controls is part of the Rolls-Royce Group


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Douglas Pauls
Sent: 26 March 2013 15:43
To: [log in to unmask]
Subject: [TN] Conformal Coat and Board Edges

OK, the conformal coat question of the day:

Do you conformally coat the edges of a printed circuit assembly?  Why or 
why
not?

OK, that is two questions, or perhaps a half fractional question.....

Doug Pauls


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________

______________________________________________________________________
This email has been scanned.

______________________________________________________________________
Aero Engine Controls is part of the Rolls-Royce Group, whose legal entity 
is
Rolls-Royce Engine Control Systems Limited which is registered in England.
Registered office at Moor Lane, PO Box 31, Derby, DE24 8BJ. Company number
6686268, UK VAT number GB 939 396 075

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________




______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2