TECHNET Archives

October 1999

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Larry Tawyea <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Thu, 21 Oct 1999 10:01:11 EDT
Content-Type:
text/plain
Parts/Attachments:
text/plain (39 lines)
Eric,

If you took a survey of everyone using electroless Ni./immersion Au., I
assume this is what you are using in the UK, 50% would say that it is fine
and 50% would say they are having solderability problems with this plating.
Some of the options that I am familiar with and should give you better
solderability are as follows;

HASL over CU, although you may have problems with thickness variations on a
micro BGA.

Immersion tin over copper, remember though that the liquidus temperature of
tin is 231C.  Eliminates the problem with HASL on thickness variations.

Electrolytic tin over copper is very solderable.  More so if it is fused to
the copper.

For high rel applications, electrolytic tin over electrolytic Ni. is also
very solderable.

Also for high rel applications an experimental plating of immersion tin over
electrolytic Ni would be very solderable.

Larry

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2