TECHNET Archives

February 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain; charset="iso-8859-1"
Sender:
Subject:
From:
Sencer Sofuoglu <[log in to unmask]>
Date:
Wed, 12 Feb 2003 09:27:02 -0600
MIME-Version:
1.0
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Sencer Sofuoglu <[log in to unmask]>
Parts/Attachments:
text/plain (146 lines)
According to paper in the Modern Electroplating book a typical Sulfamate
bath has 500psi stress while Watts bath has 18,000psi stress. Increasing
chloride concentration of Sulfamate bath increase stress to 1500psi. Is this
number too high to be low stress.  Is there a range?

Regards,

Sofu



-----Original Message-----
From: Barmuta, Mike [mailto:[log in to unmask]]
Sent: Tuesday, February 11, 2003 9:13 AM
To: [log in to unmask]
Subject: Re: [TN] electroless vs. low stress NI


Bret: One word of caution. Simply calling out electrolytic Ni does not
assure you of low stress nickel. All electrolytic Ni is not stress free.
Typically a low stress Ni electroplate is produced with a sulfamate Ni bath
and low brightners/organics. Make sure you call it out correctly


Regards

Michael Barmuta

Staff Engineer

Fluke Corp.

Everett WA

425-446-6076

-----Original Message-----
From: Adair, Bret [mailto:[log in to unmask]]
Sent: Monday, February 10, 2003 3:29 PM
To: [log in to unmask]
Subject: Re: [TN] electroless vs. low stress NI


I guess the differentiation between the two should have been electrolytic or
electroless Ni.  Thanks for the help.

Bret

-----Original Message-----
From: Crepeau, Phil [mailto:[log in to unmask]]
Sent: Monday, February 10, 2003 3:52 PM
To: [log in to unmask]
Subject: Re: [TN] electroless vs. low stress NI


hi,

for one, low stress nickel plating is associated with electro-deposited
nickel.  the bath and plating process are formulated to electrodeposit
nickel with low stresses (no duh, huh?).  for all i know, electroless nickel
deposits may have low stress also due to the fact that there ain't much
there, but it isn't referred to as 'low stress' nickel.

phil

-----Original Message-----
From: Adair, Bret [mailto:[log in to unmask]]
Sent: Monday, February 10, 2003 9:29 AM
To: [log in to unmask]
Subject: [TN] electroless vs. low stress NI


We have some prints here which call out low stress nickel followed by gold
and some call out electroless nickel followed by gold.  What is the
difference between electroless and low stress nickel?

Bret
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------


---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------


---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2