subject: pretreatment of innerlayers

to improve yields in innerlayers production, we are considering the use 
of chemical cleanning instead of pumicebrush prior to lamination of 
photoresist.
there is a new trend towards using chemical cleaning only to remove 
passivation (e.g. chromate) and impurities like organics, oxides etc.
this should be achieved by a hot alkaline spray cleaner followed by a 
ordinary acidic spray cleaner.
we are using FR4-copperclad, thickness 0,10 to 0,70 mm, copperfoil; 12 
to 70 µm. the thickness of the passivationlayer is 7,0 nm (0,007 µm).

If you have had used/or are using this new principle of pretreatment of 
innerlayers, we would like to hear what was/ is your experience with the 
process. 

best regards 
peer fisker

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2