Best use the silicon datasheet in order to get the actual tab dimensions - MO-220 only gives min/max dimensions which are
extremely wide in order to allow the actual tab to be matched to the die or allow flexibility.
If AD do not give a recommended footprint (no doubt for liability) the best recourse would be assembly house preferences or
IPC-7351.
Allegro footprint attached. No liability accepted!
Best Regards
David Greig
______________________________
GigaDyne Ltd
Buchan House
Carnegie Campus
Dunfermline KY11 8PL
United Kingdom
t: +44 (0)1383 624 975
www.gigadyne.co.uk
______________________________
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Brooks,Bill
Sent: 01 December 2005 20:52
To: [log in to unmask]
Subject: [TN] 56 pin LFCSP footprint
I have an Analog Devices part, 56-lead Lead Frame Chip Scale Package LFCSP with an 8X8mm body CP-56, supposed to be compliant
with JEDEC MO-220-VLLD-2.
Having a tough time locating a recommended footprint for this one...
Any help?
Also any issues with mounting? Since this is a direct to board soldered device, it may be subject to CTE mismatches and the
like... anyone have experience with any soldering or reliability issues with assembling this part to a fiberglass/epoxy board?
Here's a link to the part description
http://www.analog.com/UploadedFiles/Packages/352655155839944545242119821CP_5
6.pdf
<http://www.analog.com/UploadedFiles/Packages/352655155839944545242119821CP_
56.pdf>
Best regards,
Bill Brooks
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with
following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send
e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC
web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at
[log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
--
Virus scanned by Lumison.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|